Laser-Induced Damage Threshold Testing

You pick, we measure!

How do we do it?

Professional laser-induced damage threshold (LIDT) testing services are available at LIDARIS. We offer a wide range of irradiation conditions. LIDT measurements are performed in both femtosecond and nanosecond pulse duration regimes. Detailed and easy to understand measurement reports are delivered to our customers immediately after the testing. All testing procedures are conducted in accordance with guidelines of currently the latest international ISO 21254-1-2,-3 and -4 standards. Learn more about the most common and beneficial procedures below.

Non standardized testing such as R-on-1, micro-focus, rear-side and measurements in vacuum and cryogenic temperatures are available on demand. Lidaris customers get support and practical recommendations related to damage testing and optics performance either before or after testing. Also other tests and services are available on demand: Total integrated Scattering, Cavity Ring Down, Chromatic dispersion, Crystal efficiency, Transmission.

Available irradiation conditions

Download_conditions

Order process

Laser type

Pulse duration
(FWHM)(1)


Standard Wavelengths, nm

Pulse
repetition
rate, Hz

Polarization
state
AOI: 0-75°

Nd:YAG (multi-mode)
Nd:YAG (single-mode)
Nd:YAG (single-mode)
4-6 ns
10-12 ns
12-14 ns
1064 1-10
1-100
1000
Linear (S,P)
Circular
532
355
266
213
ND:YAG OPO 6-8 ns 710-810 1-100(2) Linear (S,P)
Circular
1500-2100
Yb:KGW 200 fs-
12 ps(2)
1030 Tunable 1-200000(2) Linear (S,P)
Circular
515
343
258
Ti:Sapphire(3) Tunable
40 fs-
12 ps(2)
Also 130 ps
at 800 nm
800 Tunable
1-1000
Linear (S,P)
Circular
400
266
Ti:Sapphire OPO ~40-80 fs 250-2500(4) Tunable
1-1000(2)
Linear (S,P)
Circular

Available environmental conditions

Air
(room temperature)

Available for all
irradiation conditions
Standard option
Vacuum environment Down to 10-6 mbar
Cryogenic temperatures Down to 100 K, AOI=0-60°
(1) effective pulse duration measured at Full Width Half Maximum
(2) wavelength dependent
(3) non-compressed pulses are available on demand
(4) pulse duration at wavelengths <500 nm and >1600 nm is relative between 40-80 fs
Process_download_icon7
Process_offer
Process_ship
Process_update
Process_payment
Process_results
Download Lidaris catalogue 2

Explore Laser-Induced Damage Threshold testing procedures

1-on-1 Test

1-on-1 Test

1-on-1 test is one of the simplest of laser-induced damage threshold (LIDT) determination techniques well suited for quantitative optics manufacturing process (such as coating deposition and glass polishing) optimization. Even ...

 
S-on-1 Test

S-on-1 Test

S-on-1 test procedure is most frequently used to qualify optics in terms of laser damage threshold. Most optics is intended to be used for multiple laser shots irradiation under different fluencies. ...

R-on-1 Test

R-on-1 Test

Knowledge about destructive laser damage process is essential for any type of optics in use. In some cases, testing area of the optical component is too small or not available ...

 
Laser Damage Certification

Laser Damage Certification